TECHNICAL | SOFT GROUND – HS2 PROPLESS OPENINGS - BTS MEETING
Right: Within Victoria Road Ancillary Shaft (VRAS) showing short cavern excavation to reach and expose the built rings of a running tunnel, which has been prepared for propless opening using the structural framing enabled by arrangements of special segments.
Far right: Advanced stage of connection link construction with
waterproof lining, prior to opening of the exposed rings of the running tunnel.
further shear tests on fire-tested segments. The test segments were cast in the UK and tested at Cerib facilities in France, where the laboratory built a rig that applied shear force through the middle of the connection. The supports were arranged with free rotation and deflections could be measured directly next to the joint. The second test put the specimens into a furnace. This
2020. Casting of test samples and mould delivery followed in 2021, then full testing through early 2022 in readiness for launch of NTW TBMs in late 2022 with first instalment of the special segments at an opening location soon after. Xavier handed over to Dominik to discuss structural testing of the special segment system.
Structural testing and fire performance Dominik explained that with design for the special segments was ready the project client wanted real test verification of the system performance, given then vital importance of stability and fire resistance. A testing programme around load deflection behaviour, ultimate loading and fire performance was developed. The connection has a strong direction, tangential to the
Below: Schematic showing some shafts (blue) connecting to running tunnels. The smaller shaft is a satellite ventilation shaft, positioned directly over one of the tunnels.
ring, but it also has a weaker radial direction. A question was whether the radial shear resistance was limited due to concrete breakout. With testing of some connections significantly loaded in the radial direction that performance had to be understood. Six tests for shear resistance were planned: two shear
tests in cold conditions to establish load-deflection behaviour; two fire tests under constant load; and two
was more complicated because the supports had to be insulated so they would not fail in the fire. The bearing was deliberately limited, with a small steel rod rather than a massive support, and the arrangement remained freely rotating. Four sensors measured deflection to within tenths of a millimetre next to the connection. The fire exposure was 170 minutes up to about 1,200°C.
One tested segment looked almost intact afterwards; the other looked more damaged. But the key results were the deflections from the constant load and constant shear force tests, respectively. At around 600kN, the approximately maximum force component in the weak direction, the segment performed very well during fire, with deformation of only about 1.6mm. In engineering terms, that is negligible. The more visually damaged specimen also performed well under about 1MN, approximately the maximum force in any direction, but conservatively tested in the weakest direction. Before testing, pre-assessment was carried out with
Abaqus finite element (FE) software and advanced material laws. The aim was to derive load-deflection behaviour and it was expected the limit loading would be 2MN – 3MN per connection. This is complicated modelling and cannot be done with more simplified FE software, Dominik said. The afterwards comparison with off-the-shelf
systems was clear. Standard shear connectors have limited capacity and stiffness and with conventional rebar arrangements concrete breakout limits the radial loading to approximately 200kN. By contrast, the new system design of a cast-in steel solution gave much stiffer behaviour, reaching up to 1MN-1.5MN with about 1mm of deflection, so almost nothing, Dominik said. The pieces were loaded up to around 20mm of deflection showing plastic behaviour but did not fail. The test was eventually stopped as the rig was becoming unstable, he added. The test conclusion was the very stiff, high-capacity
connection takes tension, resists fire loading and showed almost no loss of capacity after fire exposure.
14 | November 2026
Page 1 |
Page 2 |
Page 3 |
Page 4 |
Page 5 |
Page 6 |
Page 7 |
Page 8 |
Page 9 |
Page 10 |
Page 11 |
Page 12 |
Page 13 |
Page 14 |
Page 15 |
Page 16 |
Page 17 |
Page 18 |
Page 19 |
Page 20 |
Page 21 |
Page 22 |
Page 23 |
Page 24 |
Page 25 |
Page 26 |
Page 27 |
Page 28 |
Page 29 |
Page 30 |
Page 31 |
Page 32 |
Page 33 |
Page 34 |
Page 35 |
Page 36 |
Page 37 |
Page 38 |
Page 39 |
Page 40 |
Page 41 |
Page 42 |
Page 43 |
Page 44 |
Page 45