This page contains a Flash digital edition of a book.
Exploration • Drilling • Field Services


Inspection of production wells


Adam Walker reports on the latest work by a key player in specialist remote visual inspection technology.


A


n eight-year partnership on well integrity has proved extremely frutiful for all players and aptly demonstrates the merits of camera-based well inspection technology.


Te partnership has involved Inspectahire


working with Shell Global Solutions and RTD in developing visual and pulsed eddy current (PEC) inspections of production wells in the UK North Sea sector. Using small camera systems, Inspectahire has managed to get into the D annulus in several wells and find a path to the highest astronomical tide (HAT) and lowest astronomical tide (LAT). Tese areas of the surface casing and conductor have historically had the greatest wall loss. A five-year rolling programme has just been successfully completed in all Shell North Sea assets – and without any accidents or injury to personnel. Further work is now planned for TAQA and Chevron throughout 2014 as well as ongoing monitoring for Shell EPE.


cutting (100mm) into the conductor is required at two locations. A PEC probe can then be deployed down the D annulus to measure wall thickness of the surface casing and conductor if required. A further test


was developed over the years to check the integrity of the surface casing. Pressure was induced in the C annulus and cameras were lowered down the D annulus fluid level to observe. Lots of bubbles indicated large communication between annulus. Fewer bubbles indicated less communication. No bubbles and pressure build up in the C annulus indicated no communication.


Inspectahire conducted


a remote CCTV inspection of damaged conductors on a number of wells on-board a large offshore platform. Te inspection was performed during normal production conditions. All three conductors


were found to be completely sheared at the -10 support level at approximately -42m from the top of them. Te top and bottom pieces were off-set and interlocked with


Fig. 1. Illustrating how a leg entry visual inspection is conducted by Inspectahire’s advanced technology


Inspectahire believes detailed planning will result in a successful and efficient inspection, which is why a strict procedure is followed with regards to D annulus inspections. First, a thorough access survey is carried out to see if there is a sufficient gap at the top of the well between the surface casing and conductor (D annulus). Tis is done using small bullet cameras to fluid/grout level. If no access is available due to the starter head sitting on the conductor, a hole


42 www.engineerlive.com


themselves or part of the support structure. Pieces of the support structure and tulip style guide assembly appeared to be trapped between the upper and lower conductor parts. Significant wear was evident on the casing of DA-03 but could not be seen on DA-11 or DA-06 due to the casing leaning against the conductor. l


For more information ✔ at www.engineerlive.com/iog


Adam Walker is with Inspectahire Instrument Company, Aberdeen, UK. www.inspectahire.com


Fig. 2. The PEC probe can measure wall thickness of the surface casing and conductor.


Page 1  |  Page 2  |  Page 3  |  Page 4  |  Page 5  |  Page 6  |  Page 7  |  Page 8  |  Page 9  |  Page 10  |  Page 11  |  Page 12  |  Page 13  |  Page 14  |  Page 15  |  Page 16  |  Page 17  |  Page 18  |  Page 19  |  Page 20  |  Page 21  |  Page 22  |  Page 23  |  Page 24  |  Page 25  |  Page 26  |  Page 27  |  Page 28  |  Page 29  |  Page 30  |  Page 31  |  Page 32  |  Page 33  |  Page 34  |  Page 35  |  Page 36  |  Page 37  |  Page 38  |  Page 39  |  Page 40  |  Page 41  |  Page 42  |  Page 43  |  Page 44  |  Page 45  |  Page 46  |  Page 47  |  Page 48  |  Page 49  |  Page 50  |  Page 51  |  Page 52  |  Page 53  |  Page 54  |  Page 55  |  Page 56  |  Page 57  |  Page 58  |  Page 59  |  Page 60  |  Page 61  |  Page 62  |  Page 63  |  Page 64  |  Page 65  |  Page 66  |  Page 67  |  Page 68  |  Page 69  |  Page 70  |  Page 71  |  Page 72  |  Page 73  |  Page 74  |  Page 75  |  Page 76  |  Page 77  |  Page 78  |  Page 79  |  Page 80  |  Page 81  |  Page 82  |  Page 83  |  Page 84  |  Page 85  |  Page 86  |  Page 87  |  Page 88  |  Page 89  |  Page 90  |  Page 91  |  Page 92  |  Page 93  |  Page 94  |  Page 95  |  Page 96  |  Page 97  |  Page 98  |  Page 99  |  Page 100