Any weak areas on the substrate should be removed by sanding, scraping, grinding, milling, blasting or brushing. Also old, loose and weak underlayments should be removed mechanically. Surface defects such as cracks must be patched prior or during priming as there is the risk of the screed material flowing into them and producing air bubbles or reflective cracks in the surface in case of substrate movement.


Before applying subsequent floorcoverings, cement screeds are required to display a residual moisture reading of ≤ 2.0 CM-% (heating screeds ≤ 1.8 CM-%); calcium sulphate screeds: ≤ 0.5 CM-% (heating screeds ≤ 0.3 CM-%).


Sikafloor primers can be used on a wide range of substrates before the application of Sikafloor self-levelling cementitious underlayment products. The primers can reduce the absorbency of the substrates and improve the adhesion between the underlayment and the substrate.


In some cases they are also used as a protection for the substrate against the moisture coming from the self-levelling cementitious underlayments. All Sikafloor primers are rated as low-emission and meet GEV-Emicode EC-1 plus.


SUCCESSFUL MEASURES With the substrate primed and ready for its self-levelling compound, the next step is to measure the total area to be levelled in m2


. This will calculate the amount of


material necessary to achieve the mixture’s desired level and performance requirements. It’s important to note that product data sheets exclude waste and practical considerations such as surface roughness.


Whether manually or pump-applied, the water added to the levelling compound should be clear, with the quality of potable water. It is prohibited to use contaminated or waste water. When it comes to applying the self-levelling compound, proper safety equipment should be worn and sufficient ventilation provided.


The amount of water required for the levelling compound varies from product-to-product – see the relevant product data sheet. A suitable mechanical hand mixing or mixing pump is recommended for the stirring process. Never add water to the powder or add it in stages, as this alters the product’s properties.


The Sikafloor Primer and Sikafloor Level can be applied at substrate and ambient temperatures between +5°C and +30°C. Ensure all ventilation devices are switched- off during and after application for 24 hours. It’s also important to protect fresh surfaces from sunlight and direct sources of heat.


APPLYING FOR A FINISH After mixing, pour out the self-levelling compound onto the primed surface and spread using a notched trowel or adjustable pin-leveller (pinrake) to the required thickness. The compound is applied by walking along the front and keeping a ‘wet edge’; that is, always placing material onto previously placed material before it starts to set, dry (turn matt) and harden. The width of the front will be determined by the application conditions – the higher the substrate and ambient temperature, the narrower the front.


Ensure a continuous supply of mixed material and place it efficiently to allow maintaining a ‘wet edge’ which will reduce the differences between batches where the material is already starting to dry and set. Surface styling is affected by the choice of finishing tool. The use of a spike roller isn’t mandatory for every self-levelling compound, but can be recommended to remove troweling defects.


The spike rolling process should not be delayed for more than five minutes after placing, particularly at higher temperatures. A significant time-lapse could lead to roller marks, unevenness on the mortar surface or ‘waves’. Excessive rolling of the application could also cause an unsightly appearance. Depending on the thickness of the applied layer and the method of placing, the product’s ‘pot life’ and workability – usually limited to between 20 and 30 minutes at 23°C – should be decided.


Again, it’s important to reiterate that no flooring installation is the same. Mixture levels and application methods are product-dependent and likely to vary. Whatever the requirements, however, rest assured Sika offers the technical knowhow and support to ensure each self-levelling project runs as smoothly as the finished floor.


www.sika.co.uk


38 | SCREEDS, RESINS & COATINGS


www.tomorrowscontractfloors.com


Page 1  |  Page 2  |  Page 3  |  Page 4  |  Page 5  |  Page 6  |  Page 7  |  Page 8  |  Page 9  |  Page 10  |  Page 11  |  Page 12  |  Page 13  |  Page 14  |  Page 15  |  Page 16  |  Page 17  |  Page 18  |  Page 19  |  Page 20  |  Page 21  |  Page 22  |  Page 23  |  Page 24  |  Page 25  |  Page 26  |  Page 27  |  Page 28  |  Page 29  |  Page 30  |  Page 31  |  Page 32  |  Page 33  |  Page 34  |  Page 35  |  Page 36  |  Page 37  |  Page 38  |  Page 39  |  Page 40  |  Page 41  |  Page 42  |  Page 43  |  Page 44  |  Page 45  |  Page 46  |  Page 47  |  Page 48  |  Page 49  |  Page 50  |  Page 51  |  Page 52  |  Page 53  |  Page 54  |  Page 55  |  Page 56  |  Page 57  |  Page 58  |  Page 59  |  Page 60  |  Page 61  |  Page 62